The Influence of Oxidized Interlayer on the Adhesion of Bioactive Cao-P2o5-Tio2-Na2o Glass Ceramic Coating to the Titanium Substrate
Subject Areas : Journal of Environmental Friendly MaterialsSh. Honarvar 1 , B. Eftekhari Yekta 2
1 - School of Metallurgy and Materials Engineering, Iran University of Science and Technology, Tehran, Iran.
2 - School of Metallurgy and Materials Engineering, Iran University of Science and Technology, Tehran, Iran.
Keywords: Oxidation, Bonding Strength, Heat treatment, Titanium Alloys, Bioactive Coating,
Abstract :
[1] E.Verne, C. F. Valles. C. V. Brovarone, S. Spriano and C. Moisescu, J. Eur. Ceram. Soc., 24(2004), 2699.
[2] O. Albayrak, O. El-atwani and S. Altinats, Surf. Coat. Technol., 202(2008), 2482.
[3] J. Bienias, B. Suarowska, A. Stoch, H. Matraszek and M. Walczak, Dent. Mater, 25(2009), 1128.
[4] L. L. Hench, J. Am. Ceram. Soc., 74(1991), 1487.
[5] O. Yamamoto, K. Alvarez and T. Kikvhi, Acta Biomaterialia, 5(2009), 3605.
[6] T. Kasuga, T. Mizuno, M. Watanabe, M. Nogami and M. Niinomi, Biomaterials, 22(2001), 577.
[7] M. H. Fathi, A. Doostmohammadi, J. Mater. Process. Technol., 209(2009), 1385.
[8] M. Yan, C. T. Kao, J. S. Ye, T. H. H. Huang, S. J. Ding, Surf. Coat. Technol., 202(2007), 288.
[9] M. Araújo, M. Miola, A. Venturello, G. Baldi, E. Verné, J. Eur. Ceram. Soc., 36(2016)
[10] E. Cañas, M. Vicent, M.J. Orts, E. Sánchez, Surf. Coat. Technol., 318(2017).
[11] ASTM F1044 – 99, Standard Test Method for Shear Testing of Calcium Phosphate Coatings and Metallic Coatings, (2011).